Fuselage Primer

Hours this entry: 4.0
Download PDF

IMG_1525.JPG

Primered the rear half of the fuse, along with the areas that will be under the floor boards. The fuse can now be moved to hangar and continue to be worked on. Once we get the rest of the components in and set, we’ll remove them, prime the rest and paint the interior.

Just as a side note… we shot the SEM primer with a Harbor Freight HVLP gun. The gun shot fine, but after about 10 minutes the top can started leaking. I loaded the threads up with teflon tape and that solved the issue.